We have developed a process to fabricate a cross-bar structure using UV-curable nanoimprint lithography with a UV-curable double-layer spin-on resist, metal lift off and Langmuir–Blodgett film deposition. This process allowed us to produce 1-kbit cross-bar memory circuits at 30-nm half-pitch on both top and bottom electrodes. Read, write, erase and cross talking were also investigated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.