Abstract

Nanoindentation, the most widely-used probe for small-scall mechanical property evaluation, has been increasingly adopted for exploring the local behavior of shape memory alloys (SMAs). Herein, we explore the influence of the testing parameters (i.e., peak load, indenter radius, loading/unloading rate, and cyclic loading) on the superelastic behavior of a Ni-Ti SMA at room temperature, at which it is in the austenitic state, during spherical nanoindentation. The possible underlying mechanisms for measured response due to each of the testing parameters are discussed in terms of the roles of forward/reverse stress-induced phase transformations, dislocation activity, latent heat evolution, and geometric compatibility of the interfaces during the post-yield deformation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.