AbstractZn0.5Ni0.5-xCoxFe2-yLayO4 ferrites (with x=0, 0.02 and y=0, 0.02) were prepared by an industrial method using the standard ceramic technique and sintered at 1,250°C in air. X-ray diffraction (XRD) was used to obtain the phase formation of the NiZn ferrites. The microstructure of ferrites was investigated by scanning electron microscopy (SEM). The XRD reveals that lattice parameter (a) is decreased and a secondary phase (LaFeO3) is formed in the La–Co co-substituted NiZn ferrite sample, meanwhile, the grain size (D) of this sample decreased obviously by observing SEM photographs. Vibrating sample magnetometry (VSM), B-H analyzer, impedance analyzer and electrometer were carried out in order to characterize some properties of the ferrites. This investigation indicates that, La–Co co-substituted NiZn ferrite sample has higher power loss (Pcv) than other samples at low frequency with an increase in coercive field (Hc) and magnetocrystalline anisotropy (K1), a decrease in initial permeability (μi) and saturation magnetization (Ms). However, at high frequency, the power loss of La–Co co-substituted sample is low, which is attributed to high resistivity (ρ), small grain size (D), less number of Fe2+ ions and low porosity (P).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.