Abstract

Polyvinyline fluroide- CaCu3Ti4O12 (PVDF-CCTO) nanocomposite films have been fabricated by solution casting method, where CaCu3Ti4O12 (CCTO) nanopowder is incorporated in PVDF polymer matrix. Synthesized films have been structurally, morphologically, and electrically characterized. Dielectric constant of PVDF-CCTO nanocomposite is found to increase with increase in loading of CCTO nanopowder in the frequency range 100 Hz - 1 MHz. Obtained dielectric constant of composites has also been fitted in various theoretical models. Unlike dielectric behaviour, polarization does not show the ordered variation with the loading of CCTO nanopowder. PVDF-CCTO nanocomposite with 8 vol% of CCTO exhibits highest saturation and remnant polarization 1.7 μC/cm2 at 500 kV/cm and 0.6 μC/cm2, respectively. It also possesses highest discharge energy density 0.85 J/cc at 500 kV/cm and energy efficiency of ~65% at 100 kV/cm. Enhanced energy density and polarization are attributed to increase dipole moment due to ordering of α, β, γ-phases of PVDF in PVDF-CCTO nanocomposite films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.