Abstract

An aqueous sol–gel synthesis route has been used for the preparation of undoped and cerium-doped strontium aluminate phase Sr4Al14O25. This study revealed required conditions for obtaining single phase compound, which are 1300°C annealing temperature and addition of 2.5% of boric acid as a fluxing agent. The fact that boric acid is involved in the process of formation of strontium aluminate was confirmed by thermogravimetric measurements. A series of cerium-doped samples has been prepared and their excitation and emission spectra has been measured, which showed peaks at 330nm and 385nm, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.