Abstract
ABSTRACT Machining cracks in ground sintered reaction-bonded silicon nitride (SRBSN) rods and bars were analyzed by fractographic techniques. Grinding flaw sizes were as small as 12 µm and as large as 80 µm and correlated strongly with grinding direction and wheel grit size. Some grinding treatments had no deleterious effect on strength since the machining cracks were very small and fracture occurred from the material's inherent flaws. The telltale signs of machining damage may be detected with conventional low power optical microscopy using simple fractographic techniques. The telltale signs are summarized in a new series of schematic drawings which will aid pattern recognition for engineers and fractographers.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.