Abstract

The secondary reaction zone (SRZ) formation at the interface between CoNiCrAlY coating and experimental Ni-based single-crystal superalloy substrate with 1 wt.% Ru has been investigated. The γ′ grains nucleated epitaxially with grains in coated layer. Preferential formation of the SRZ was observed along the 〈1 1 0〉 directions. The factors affecting the SRZ kinetics are discussed in terms of the preferential dislocation gliding direction where recrystallization would be most active due to high strain energy and the supply of fast interdiffusion pathways.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.