Abstract
Abstract The present investigation describes the kinetics of γ-channel widening in the single-crystal superalloy CMSX-4 at temperatures above 1000 °C and at stress levels between 50 and 100 MPa. A miniature tensile creep specimen (uniaxial loading in 〈0 0 1〉-direction) and a double shear creep specimen (biaxial loading of the macroscopic crystallographic shear system {0 1 1} 〈0 1 1 〉 ) were used for interrupted creep testing. The volume fractions of the γ- and γ′-phases and the kinetics of γ-channel widening were investigated using high resolution scanning electron microscopy in combination with quantitative metallography. It was found that rafting always occurred perpendicularly to the direction of the maximum principal stress (i.e. perpendicular to the tensile direction in the tensile specimens and in 45° to the shear stress for the shear tests). Over the whole stress range, there was no significant difference between γ-channel widening in 〈0 0 1〉-tension and {0 1 1} 〈0 1 1 〉 -shear creep deformation, when the experiments were performed at the same maximum principal stress. γ-Channel widening is an important process during creep of γ/γ′-microstructures because dislocations propagate in the thin γ-channels. Our present study shows how temperature, stress level and stress state affect this microstructural coarsening process. Superimposed stresses favour the γ-phase, and therefore channel widths increase faster with increasing superimposed stresses.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.