Abstract
Temperature-modulated differential scanning calorimetry (TMDSC) is based on conventional DSC but with a sinusoidally modulated temperature path. Simulations of TMDSC signals were performed for Corning EAGLE XG glass over a wide range of modulation frequencies. Our results reveal that the frequency correction commonly used in the interpretation of TMDSC signals leads to a master nonreversing heat flow curve independent of modulation frequency, provided that sufficiently high frequencies are employed in the TMDSC measurement. A master reversing heat flow curve can also be generated through the frequency correction. The resulting glass transition temperature from the frequency corrected reversing heat flow is thereby shown to be independent of frequency.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.