Abstract

Cold-drawn pearlitic steel wires are widely used in numerous engineering fields. Combining X-ray line profile analysis and positron annihilation spectroscopy methods, up to 10−5–10−4 vacancies were found in α-ferrite of a cold-drawn pearlitic steel wire with a true strain of e = 3. The formation of deformation-induced vacancies in α-ferrite of cold-drawn pearlitic steel wire was quantitatively testified.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.