Abstract

CdS films were prepared by a physical vacuum deposition technique on an amorphous (glass) substrate using a modified evaporation source. The effect of the processing conditions (the film thickness, substrate temperature and the deposition rate) were considered in comparison with the normal evaporation source. A van der Pauw four-probe arrangement was used for measuring the electrical resistivity, which varies between 0.1 × 104 and 8.18 × 104Ωcm. It decreases with increasing film thickness, and decreasing deposition rate and substrate temperature. This was attributed to the effect of crystallite size, the degree of preferred orientation, internal microstrain and the stoichiometry. From spectrophotometric measuring and using an approximate formula, the optical parameters (n,k, α) were evaluated. The values of the refractive indices and the energy gaps were evaluated and correlated with the preparation parameters.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.