The role of boron in conferring the grain boundary character in a new polycrystalline superalloy suitable for power generation applications is considered. One boron-free and three boron-containing variants are studied using a suite of high resolution characterisation techniques including atom probe tomography (APT), high resolution secondary ion mass spectroscopy (SIMS) and transmission electron microscopy (TEM). The primary effect of boron addition is the suppression of Cr-rich M23C6 carbide and the formation instead of the Cr-rich M5B3 boride. The SIMS analysis indicates that the boride particles are distributed fairly uniformly along the grain boundaries, of length up to 500 nm along the grain boundary. The substantial majority of the boron added resides in the form of these M5B3 borides; some boron segregation is found at the γ′/M5B3 interfaces but interfaces of other forms – such as γ/γ′, γ/M5B3, γ/MC and γ′/MC – show no significant segregation. Creep testing indicates that the optimum boron content in this alloy is 0.05 at.%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.