Abstract

A new hypothesis for formation of non-propagating cracks under fatigue of metals is proposed. The hypothesis is based on coaxing effect and strain hardening effect and others, which the related material receives at the tip of a fatigue crack. Due to these effect, the material at the tip of fatigue crack is considered to be stronger at inner parts than at near surface. The fatigue strength for formation of cracks and that for destruction are considered. A critical value of the fatigue strength reduction factor, which means the minimum value of it for formation of non-propagating crack, is also considered. The relation between the critical fatigue strength reduction factor and the fatigue strength of two kinds above mentioned is obtained from the hypothesis proposed. The reduced relations are compared with the results of experiments made on rotating bending and repeated torsion, and a good agreement is noticed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.