Abstract

Differential scanning calorimetric (DSC) measurements have been made in glassy Se 70Te 30− x Ag x alloys. At low concentration of Ag ( x = 2, 4, 6), only one endothermic and one exothermic peaks are observed at glass transition and crystallization temperatures. However, at higher concentration of Ag ( x = 8, 10), two endothermic and two exothermic peaks have been observed in DSC scans. The double stage crystallization at higher concentration of Ag has also been reported in various other glassy systems by other workers. The activation energy of crystallization ( E c) has been determined for each stage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.