Abstract

The structure and composition of passive film formed on Fe–20Cr–xNi (x=0, 10, 20wt.%) alloys in deaerated pH 8.5 borate buffer solution was examined by transmission electron microscope and Cs-corrected scanning transmission electron microscope-electron energy loss spectroscopy. Thickness of the passive film on each alloy was measured to be 2.5–2.7nm and the passive film was enriched with Cr. The passive film formed on the alloys exhibited an amorphous structure, as confirmed by the lack of diffraction contrast and by the fast Fourier transform images taken within a region of the passive film on each alloy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.