Acoustic oscillations were observed in ultrafast transient absorption of nanostructured Ag films produced by plasma-enhanced atomic layer deposition (PEALD). The oscillations are attributed to modulations of localized surface plasmon resonance (SPR) bands that naturally arise in the PEALD films and can be described as two lateral modes (∼50 and 100 GHz) with different dephasing times. Contributions from electron-phonon coupling and lattice dynamics in the transient response vary systematically with the probe wavelength relative to the SPR maximum (500–1000 nm).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.