Abstract

The thermal metallurgical modeling of alloying aluminum redistribution was further developed through couple of heat transfer model, dendrite selection model, multicomponent dendrtie grwoth model and nonequilibrium solidification model during three-dimensional nickel-based single-crystal superalloy weld pool solidification over a wide range of welding conditions (laser power, welding speed and welding configuration) to facilitate understanding of solidification cracking phenomena. It is indicated that the welding configuration plays more important role than heat input in aluminum redistribution. The bimodal distribution of solid aluminum concentration along the solid/liquid interface is crystallographically symmetrical about the weld pool centerline for (001) and [100] welding configuration, while the distribution of solid aluminum concentration along the solid/liquid interface is crystallographically asymmetrical throughout the weld pool for (001) and [110] welding configuration. The size of vulnerable [100] dendrite growth region is beneficially suppressed in favor of epitaxial [001] dendrite growth region through optimum low heat input (low laser power and high welding speed) to facilitate single-crystal dendrite growth for successful crack-free weld at the expense of shallow weld pool geometry. The overall aluminum concentration in (001) and [100] welding configuration is significantly smaller than that of (001) and [110] welding configuration regardless of heat input. Severe aluminum enrichment is confined to [100] dendrite growth region where is more susceptible to solidification cracking. Heat input and welding configuration are optimized in order to minimize the solidification cracking susceptibility and improve microstructure stability. The relationship between welding conditions and alloying aluminum redistribution are established for solidification cracking susceptibility evaluation. The higher heat input is used, the more aluminum enrichment is monotonically incurred by diffusion with considerable increase of metallurgical driving forces for morphology instability and microstructure anomalies to deteriorate weldability and vice versa. The mechanism of asymmetrical solidification cracking because of crystallography-dependent alloying redistribution is proposed. The theoretical predictions agree well with the experiment results. Moreover, the useful modeling is also applicable to other single-crystal superalloys with similar metallurgical properties during laser welding or laser cladding.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.