Abstract
Nucleation mechanism of a nickel-base superalloy during dynamic recrystallization Shuai WANG , Lei WANG 1)∗, Yang LIU , Guohua XU , Beijiang ZHANG 2) and Guangpu ZHAO 2) 1) Key Laboratory for Anisotropy and Texture of Materials, Northeastern University, Shenyang 110819, China 2) High Temperature Materials Research Institute, Central Iron and Steel Research Institute, Beijing 100081, China Manuscript received 24 August 2010; in revised form 11 November 2010
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.