Elemental depth profiling by glow discharge optical emission spectroscopy has been used to characterize the corrosion products on AA2024‐T3. In previous work, the aluminium, oxygen and copper depth profiles were shown to provide information regarding surface roughening, the thickness of corroded layers and extent of copper de‐alloying/relocation. Nitrogen, sulfur, phosphorus and chromium depth profiles were examined in the hope of detecting inhibitor species within the corroded/altered layers after 5 h of exposure to a corrosive solution. In the present work, the study is extended to longer exposure time. The work presents a further study of the leaching of benzotriazole from the coating matrix or from nanocontainers during various times of exposure to a corrosive environment. Copyright © 2016 John Wiley & Sons, Ltd.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.