Abstract
Powder packing behavior plays an important role in determining sintering ability of powder and the resultant performance of materials. In this study, a novel powder packing theory with bimodal particle size distribution is proposed by considering the loosening effect, wall effect and wedging effect. This theory is applied in PM nickel base superalloy by using mixture of coarse particles and fine particles. Microstructures of alloy sintered by vacuum hot pressing (HP) are observed by optical microscope (OM) and electron backscatter diffraction (EBSD). The prediction result by this theory is in good agreement with the experimental results. The enhanced sintering ability of powder containing appropriate fractions of coarse particle and fine particle is ascribed to the filling of fine particles to the voids between coarse particles, which enhanced the density of sample after sintering. Tensile behavior and the fracture morphology of alloys with various particle distributions are analyzed in details, suggesting the higher reliability of the present theory.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.