Abstract

AbstractLiK7[Li3SiO4]8:Eu2+ (LKLSO:Eu2+) was synthesized by a high‐temperature solid‐state reaction. It is accessible from K2CO3, Li2O, SiO2, and an Eu‐source (Eu2O3) by conventional solid‐state reaction in nickel crucibles under a constant flow of forming gas. The crystal structure of LKLSO has been determined by single‐crystal X‐ray diffraction and it crystallizes in the tetragonal space group I (no. 88) with the lattice parameters a=1560.83(5), c=1278.23(4) pm, and a volume of V=0.31140(2) nm3. The compound is isostructural to NaK7[Li3SiO4]8:Eu2+ but, in contrast, features an enhanced suppression of the second broad band emission through the specific channel filling in the crystal structure. Despite the observed positional disorder in the structure, the cyan‐green phosphor shows a narrow band emission with a maximum at 511 nm and a fwhm of 45 nm (0.215 eV).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.