Abstract
Abstract The AAO membrane was modified by immersion within Zn(NO3)2 solution. Zinc-containing film would be formed over the inner surfaces of membrane. Using this as template, ZnO film-coated carbon nanotube arrays were fabricated in plasma-enhanced CVD.