Abstract

AbstractThis paper describes the synthesis of amphiphilic block copolymers by living radical polymerization (NMP) of new styrene‐like monomers. The polar monomers (ethylene oxide side chains and free hydroxyl‐ or amino‐groups after deprotection) were polymerized in a “protected form” to adjust the solubility of the monomers. In this way high molar mass polymers with a narrow polydispersity (around or below 1.2) were accessible. In the bulk state hydrophobic and hydrophilic domains demix. By exposing thin films of these polymers to vacuum (air) or alternatively to water or a hydrophilic surface it becomes possible to switch the surface polarity reversibly between contact angles of about 105° and 83° as a result of surface reconstruction. Through side chains of different length and with different functionalities, it was possible to adjust the glass transition temperatures to values between −2 °C to 140 °C for the hydrophilic blocks and −30 °C to 100 °C for the hydrophobic block. The wide range of the glass temperatures allowed it to find a block copolymer system with a slow kinetic concerning the surface reconstruction process, so that a mechanistic examination of the process by AFM was possible. It got, thereby, possible to detect the break‐up of the hydrophobic surface lamella and the upfold of the hydrophilic lamella in contact with water.magnified image

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.