Abstract

At 700 K, the optimal ZT of SnNCl and SnNBr monolayers reached 2.55 and 3.23, respectively. Higher ZT values and good ferroelasticity indicate that SnNX (X = Cl, Br) monolayers should be promising thermoelectric and ferroelastic materials.