Abstract
AbstractA new nonlocal damage‐viscoplastic model for high temperature creep of single crystal superalloys is developed. It is based on the variational formulation consisting of free energy, plastic and damage dissipation potentials. Evolution equations for plastic strain and damage variables are derived from the minimum principle for dissipation potentials [1]. The model is capable of describing different stages of creep in a unified way. The evolution of dislocation densities of gamma and gamma prime phases in superalloys incorporates plastic deformation. It results in the time‐dependence of the creep rate in primary and secondary creep. Tertiary creep is taken into account by introducing local and nonlocal damage variables. Herein the nonlocal one is considered as numerical treatment to remove mesh‐dependence. Numerical results and comparisons with experimental data of the single crystal superalloy LEK94 are shown. (© 2011 Wiley‐VCH Verlag GmbH & Co. KGaA, Weinheim)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.