Abstract

A composite liner of carbon phenolic has been inspected by ultrasonic, X-ray radiography andX-ray computed tomography (CT) to find defects like delaminations, debonds, voids, foreign inclusions, etc.The geometry, detection of multiple defects and porosity of the liner make ultrasonic testing (pulse-echo anddrycoupling) difficult for inspection. X-ray radiography being a non-contact technique finds multiple defectsbut compresses the structural information of 3-D volume into a 2-D image and interferes with overlyingand underlying areas of the object. X-ray CT generates an image of a thin and cross-sectional slice ofan object. R e linear attenuation coefficients in terms of Hounsfield values have been measured, comparedand correlated with CT images at the contrasts observed. 3-D images can be generated by stacking2-D cross-sectional images of the slices. These 3-D images can be cut at any angle of choice for mappingthe extent of delaminated/debonded areas. This type of information is difficult to obtain with conventionalnon-destructive testing techniques.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.