According to the present knowledge the non-proportionality of the light yield of scintillators appears to be the fundamental limitation of energy resolution. Thus, the understanding of its origin is of the great importance for a development of new scintillators with enhanced energy resolution. In this respect, the non-proportional response of the typical organic scintillators was studied in comparison to that of a BGO crystal. The studies covered tests of BC408 plastic, BC501A liquid scintillator and anthracene organic crystal. The measurements showed a much larger range of energies presenting non-proportional response compared to that known for inorganic scintillators. In the case of anthracene the non-proportionality covers energy range up to about 500 keV, while for the BC408 plastic and BC501A liquid scintillators, it is above 4 MeV energy lost by gamma quanta. The observed effect can be related to a strong quenching of the light for charged particles in organic scintillators, which is much larger than that observed in inorganic scintillators.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.