Zn 0.96Mn 0.03Al 0.01O powders have been synthesized using the co-precipitation technique. X-ray diffraction patterns show the typical würtzite structure with no additional peaks for all samples. Raman spectroscopy revealed that Mn 2+ ions were substituted for Zn 2+ into the ZnO matrix and that Al and Mn ions activate an additional vibration mode at 670 cm − 1 which is specific to interstitial defects. The resistance measurements give a confirmation of the presence of free carriers. Nevertheless, magnetization measurements revealed only a mixture of paramagnetic and antiferromagnetic behaviors for all samples with no sign of ferromagnetism.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.