Abstract

Meta- and para-diethyl-p,p-oxydiphenylene pyromellitamide (DOP), the model compounds of the meta and para PMDA/ODA polyamic ethyl ester, were synthesized and characterized by NMR and FTIR spectroscopy. Investigation of the imidization in d6-DMSO solution using NMR and FTIR techniques has shown that both the half imide and imide were formed. Quantitative analysis of the curing rates and degrees of conversion of the isomers in dilute d6-DMSO solution as a function of time under isothermal conditions or as function of temperature at fixed time (1 h) indicated that the kinetics of the ring closure reaction of the meta and para isomers were the same within 10%. This suggests that intrinsic reactivity differences between the isomers do not have much effect on the imidization process and do not account for the differences in rate that have been observed for the meta and para polymers in the solid state. No interconversion between the two isomeric forms occurred below 180°C, as has been observed for polyamic acids and their model compounds. The degree of conversion strongly depended on the reaction temperature and increased quickly after 170°C. The rate constant of the second ring closure reaction was found to be approximately three to four times the rate constant of the first ring closure reaction. © 1996 John Wiley & Sons, Inc.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.