Three different methacrylic monomers (γ‐butyrolactone methacrylate (GBLMA), 3‐hydroxyl‐1‐adamantyl methacrylate (HAMA), and 2‐methyl‐2‐adamantyl methacrylate (MAMA)), that are most often terpolymerized for 193 nm photoresists, were studied individually by nitroxide mediated polymerization (NMP) with succinimidyl ester terminated BlocBuilder (NHS‐BlocBuilder) using a small fraction ∼ 0.05 mol/mol (5 mol%) in the initial mixture of 2,3,4,5,6 pentafluorostyrene (PFS) controlling co‐monomer. The copolymerizations were done in 0.35 g/g (35 wt%) dioxane solution and were studied as functions of temperature (75 versus 90 °C) and added free SG1 nitroxide (none versus SG1:NHS‐BlocBuilder molar ratio ≈ 0.15) with the objective of minimizing the dispersity (). MAMA/PFS copolymerizations were not strongly influenced by temperature or addition of free nitroxide, with relatively linear number average molecular weight versus conversion plots and = 1.28–1.55. Further, MAMA/PFS polymerization kinetics was notably slower compared to GBLMA or HAMA copolymerizations with PFS. For GBLMA/PFS and HAMA/PFS copolymerizations, was reduced at the lower temperature of 75 °C but added SG1 did not play a strong role. For GBLMA/PFS, was reduced from 1.70–1.71 at 90 °C to 1.42–1.50 at 75 °C and for HAMA/PFS, was reduced from 1.36–1.47 at 90 °C to 1.22–1.31 at 75 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: The Canadian Journal of Chemical Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.