Abstract

The nitrogen solubility in liquid Fe-Mn and Fe-Mn-Al alloys has been measured by the gas-liquid metal equilibration technique utilizing a high frequency induction furnace under the nitrogen partial pressures of 0.1 to 0.8 atm in the temperature range of 1773 to 1873 K. The variation of the nitrogen solubility with the addition of manganese was measured by sampling and in-situ analysis of nitrogen content. Manganese significantly increased nitrogen solubility in liquid Fe-Mn and Fe-Mn-Al alloys. The nitrogen dissolution followed the Sieverts’ law for liquid Fe-Mn alloys contained manganese up to 26 mass%. Using the Wagner’s interaction parameter formalism, the experimental results were thermodynamically analyzed to determine the first- and second-order interaction parameters of manganese and aluminum on nitrogen in high Mn-Al alloyed liquid steels. No temperature dependence of these values was observed in the temperature range of 1773 to 1873 K. eNMn = −0.023, rNMN = 0 rNMn,Al = 0 (Mn≤26 mass%, Al≤0.4 mass%, 1773–1873 K).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.