A Ni/NiFe2 dual-layer coating is deposited on 50-h pre-oxidized SUS 430 steel by magnetron sputtering for solid oxide fuel cell (SOFC) interconnects application, followed by thermal exposure in air at 800 °C for 1680 h. The thermally grown oxide scales exhibit tri-layer structure with inner Cr2O3 layer, middle NiO layer and outer NiFe2O4 spinel layer. The oxide coating converted from Ni/NiFe2 coating not only inhibit the growth of Cr2O3 and the outward diffusion of Cr species but also improve the electrical performance of the surface scale. In addition, pre-oxidation treatment for the steel before Ni/NiFe2 coating deposition prevents the interdiffusion between steel substrate and coating in the oxidation process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.