Abstract

MgAl 2O 4 spinel oxide-supported Ni catalysts modified with Pr have been prepared by wet impregnation method with 8 wt.% Ni and variable loadings of Pr (0–7 wt.%). The samples were characterized by ICP, BET, XRD, TPR, SEM, Raman and TG-TPO and they were tested in ethanol steam reforming reaction. The XRD of the samples revealed the presence of spinel phase MgAl 2O 4, NiO and weak lines of PrO 2/Pr 6O 11. The addition of Pr slowed down the deactivation rate affecting the amount and the type of carbon deposit. Under reactive conditions, the system with 2.6 Pr wt.% showed the best performance and although it presented filamentous carbon, this catalytic system kept around 80% ethanol conversion during the reaction time (40 h) under severe reforming conditions without reactor plugging.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.