Abstract

Zircon-manganites of the composition LaMeI2ZrMnO6 (MeI – Li, Na, K). were synthesized using the ceramic technology method in the range of 800-1200°C by the interaction of lanthanum (III) oxides and lithium, sodium and potassium carbonates (analytical grade). Using X-ray diffraction methods, it was established that all synthesized zircon-manganites crystallize in a cubic system with the following lattice parameters: LaLi2ZrMnO6 – а = 16,26 ±0,02 Å; V0 = 4300,93 ±0,06 Å3; Z = 6; V° elem cell = 716,82 ± 0,02 Å3; r x-ray. = 5,49 g/сm3; r picn. = 5,42 ± 0,06 g/сm3; LaNa2ZrMnO6 – а = 16,85 ± 0,02Å; V0 = 4785,46 ± 0,02 Å3; Z = 6; V° elem cell = 795,58 ± 0,02 Å3; r x-ray. = 5,35 g/сm 3; r picn. = 5,30 ± 0,04 g/сm 3; LaK2ZrMnO6 – а = 17,45 ± 0,03 Å; V0 = 5318,85 ±0,09 Å3; Z = 6; V° elem cell = 885,81 ± 0,02 Å3; r x-ray. = 5,16 g/сm 3; r picn. = 5,08 ± 0,02 g/сm 3. It has been established that with an increase in ionic radii in the Li®Na®K series, the values of the parameter “a” and the volumes of lattices and unit cells of zircon-manganites increase.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.