Abstract

In this work a new ultra-high temperature (UHT) nanoindentation system for testing at up to 1100 °C is presented. The system is capable to perform indents from small scale up to large indentation depths due to the combination of a 1 N actuator and a frame stiffness of >1·106Nm even at 1100 °C. Dynamic testing allows a continuous determination of the contact stiffness (CSM) and thus also the depth-dependent hardness and indentation modulus. Low drift rates can be achieved by an independent tip and sample heating. Operating the nanoindenter inside a scanning electron microscope (SEM) equipped with a high temperature backscattered electron (BSE) detector opens the possibility of in-situ observations, as high vacuum minimizes oxidation effects. The HT capability of the system is demonstrated on three reference materials: fused silica, molybdenum assessing the change in modulus with increasing temperature using constant strain rate tests (CSR). The creep response of single crystalline Ni has been assessed by strain rate jump (SRJ) as well as a step-load and hold creep (SLH) method. The resulting modulus, hardness as well as the strain rate sensitivity from RT up to 1100 °C are in good accordance with literature data, highlighting the applicability of the system.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.