Abstract

Repairing skin wounds has always been challenging in clinical practice. The new skin tissue engineering scaffold provides innovative ways to address these challenges with a good chance of success because of its stable mechanical properties, biodegradability, and antibacterial properties. This paper presents the fabrication and evaluation of a three-dimensional composite scaffold made with sulfated silk fibroin, chitosan, and hydroxyapatite (SSF/CS/HAP). An electron microscope shows that the scaffold has an aperture of 15–20 μm, while an absorption performance test shows that its expansion index reaches 779%. The co-culture of L929 cells and the CCK-8 experiments demonstrated good cell compatibility and low scaffold cytotoxicity, respectively. Meanwhile, in vivo experiments demonstrate that rats with SSF/CS/HAP scaffold-treated neck wounds heal faster. In the wound skin tissue of the SSF/CS/HAP scaffold group, immunohistochemistry indicates a more rapid and mature development of hair follicles. This study successfully developed a novel skin tissue engineering scaffold material with high moisture retention, high tissue compatibility, and low cytotoxicity, demonstrating its ability to improve wound repair with promising potential for tissue engineering applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.