Abstract

Two new hydrogenic shallow donors with binding energies of 38.32 and 40.09 meV are observed, in addition to phosphorus (P) and antimony (Sb) donors, in n-type high-purity silicon crystals by means of high-resolution photothermal ionization spectroscopy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.