Abstract
The present paper analyzes the differences in behavior and resistance to erosion through vibrating cavitation, between the bronze structures CuSn-12C resulting from two volumetric thermal treatments of hardening and tempering. The analysis was performed on the basis of macro and microscopic images, as well as on the basis of the histogram in which the values of the reference parameters used in the laboratory custom and prescribed by the international norms ASTM G32-2016 are compared. This shows the dependence of the degree of erosion as a function of the temperature of tempering heat treatment, after hardening, as a result of microstructural changes and the hardness of the surface attacked by cavitation. The experimental research is performed on the standard vibrating device within the Cavitation Erosion Research Laboratory of the Politehnica University of Timișoara.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.