Abstract
Silicon-containing coatings with a matrix consisting of the saturated γ solid solution Ni 6Cr 2Si 2 and which also contain intermetallics of complex tantalum silicides as precipitates show great promise as protective layers for nickel-based alloys with improved oxidation and hot corrosion resistance. We present results of oxidation tests performed at 1000°C for up to 4000 h in air and of hot corrosion tests in burner gas with intermediate dipping in Na 2SO 4 and V 2O 5 melts. From silicon diffusion data, lifetimes greater than 10 000 h at 1000°C can be expected.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.