Abstract

In the Pb(Zr, Ti)O3 group ceramics, the dielectric loss becomes larger than the mechanical vibration loss under high-power excitation. In this paper, a new advanced method for measuring these losses separately and simultaneously is described. The two-step differential circuit is utilized. By adjusting the differential circuits, the dielectric loss and the damped capacitance are obtained. The resonance circuit constants under high-power excitation are obtained after adjusting the differential circuit.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.