We found the most promising powder material for the application of the thermal coagulation therapy for the treatment of cancerous tissues. The maximum heat generation ability (ΔT = 40–77 °C, 370 kHz, 1.77 kA·m − 1 ) was obtained for the powder materials by the calcination at 1100 °C for the Y 3 − X Gd XFe 5O 12 system. This ΔT value is higher than ca. ΔT = 30 °C in same magnetic field for fine FeFe 2O 4 particles as the candidate material for this type of therapy. The particle growth with the formation of the cubic single phase might influence to the high heat generation. As an unexpected result, the Gd 3Fe 5O 12 (X = 3) has no heat generation ability in an AC magnetic field.