Abstract

We optimized synthesis conditions of blue-emitting CaMgSi2O6:Eu2+ (CMS:Eu2+) with conventional solid-state reaction and successfully determined structure parameters by Rietveld refinement method with neutron powder diffraction data. The final weighted R-factor Rwp was 6.42% and the goodness-of-fit indicator S (= Rwp/Re) was 1.34. The refined lattice parameters of CMS:Eu2+ were a = 9.7472(3) Å, b = 8.9394(2) Å, and c = 5.2484(1) Å. The β angle was 105.87(1)°. The concentration quenching process was observed, and the critical quenching concentration of Eu2+ in CMS:Eu2+ was about 0.01 mol and critical transfer distance was calculated as 12 Å. With the help of the Rietveld refinement and Dexter theory, the critical transfer distance was also calculated as 27 Å. In addition, the dominant multipolar interaction of CMS:Eu2+ was investigated from the relationship between the emission intensity per activator concentration and activator concentration. The dipole–dipole interaction was a dominant energy transfer mechanism of electric multipolar character of CMS:Eu2+.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.