Abstract

To understand the microstructural stability of candidate plasma-facing materials under fusion-relevant environments, neutron irradiation of W and W-3%Re alloys with and without K and La dopants was performed in the mixed-spectrum High Flux Isotope Reactor at nominal temperatures of ~850 °C and ~1100 °C to calculated doses between 0.42 and 0.47 dpa. To the best of our knowledge, this study presents the first experimental evidence of radiation-enhanced recrystallization in W and undoped W–Re alloys at ~850 °C, conditions where thermal annealing does not cause any grain growth in a similar timescale. Potassium- or lanthanum-doped tungsten alloys showed more resistance to radiation-enhanced grain growth. We explain the acceleration of grain growth by analyzing the self-diffusion constant under atomic displacement environments. The microstructural observations of the studied W variants suggest that La doping is more effective than K doping for mitigating recrystallization. This study also found that radiation-enhanced recrystallization is an important consideration when designing and applying W to plasma-facing components in future nuclear fusion reactors.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.