Abstract

Solid solutions Nd2−xSrxNiO4±δ (x = 0, 0.5, 1, 1.2, 1.4) with a K2NiF4 structure can be obtained from freeze-dried precursors. The end members of this series can be obtained at T ≥ 1000 °C only, while complex oxides with x = 1; 1.5 are formed at T ≥ 700 °C. Thermal analysis revealed the two stages of Nd2−xSrxNiO4±δ thermal reduction in a 10%H2/Ar gas mixture that was completed at 900 °C. For x < 0.2, the reduction products demonstrated an exsolution-like morphology with Ni nanoparticles allocated at the surface of oxide grains. As-obtained nanocomposites with x = 0 and x > 1 revealed the outstanding catalytic activity and selectivity in the dry reforming of the methane (DRM) reaction at 800 °C with CH4 conversion close to the thermodynamic values. The appearance of two different maxima of the catalytic properties of Ni/(Nd2O3,SrCO3) nanocomposites could be affiliated with the domination of the positive contributions of Nd2O3 and SrCO3, respectively.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call