Abstract

The two compositions Al 70Co 15Ni 15 and Al 65Cu 20Co 15 forming decagonal phases in both as-cast and rapid solidification conditions display subtle differences in their diffraction patterns. We present here the structural investigation of a series of alloys in Al–Co–Cu–Ni system under rapid solidification conditions. Many interesting structural features giving rise to subtle differences in the nature of streaking and also diffuse intensity will be discussed. An attempt will be made to correlate these effects with the chemistry of the alloy. The observation of diffuse intensity leading to the change in symmetry from P10 5/mcm to 10/mmm will be considered in terms of statistical occupancy of various components constituting the above systems.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.