Abstract
Abstract NASA developed a novel oxide dispersion strengthened (ODS) NiCoCr-based alloy, GRX-810, that exhibits exceptional high temperature properties compared to conventional wrought superalloys for 3D printing applications. In this interview, the co-inventors, Tim Smith and Christopher Kantzos, discuss the alloy's unique development process and its superior high strength and durability for aerospace and other extreme conditions.