Abstract

We report on the modification of the local coordination of Cu in TiN–Cu films, as a function of the growth conditions. The films were deposited on Si (100) by pulsed laser deposition using either an intermetallic TiCu target or elemental Ti and Cu targets. During growth the partial nitrogen pressure (p(N 2)) took values in the range 0–150 ⋅ 10 − 3 mbar. The bonding environment of Cu is identified using Extended X-Ray Absorption Fine Structure Spectroscopy (EXAFS) measurements at the Cu- K-edge. It is disclosed that in the films grown under p(N 2) < 150⋅10 − 3 mbar, Ti partially substitutes Cu in the fcc Cu phase. However, both the Cu–Ti bondlength and the coordination of Cu in the 1st nearest neighbor shell change as a result of the different growth conditions. More specifically, in the films grown in N 2 ambient, the degree of incorporation of Ti in fcc Cu sites decreases as the p(N 2) increases. When growth occurs from elemental targets under p(N 2) = 150 ⋅ 10 − 3 mbar, only fcc Cu is detected. The changes in the coordination of Cu as a function of the p(N 2) are attributed to the formation of crystalline TiN. Finally, the Cu–Cu bondlength is equal to the respective bondlength in the Cu-foil, independent of the growth conditions while, on the contrary, the Cu–Ti bondlength depends on p(N 2).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.