AbstractWe used thin‐film differential scanning calorimetry to investigate the melting of isolated polyethylene single crystals with lamellar thicknesses of 12 ± 1 nm. We observed the melting of as few as 25 crystals. Over a wide number of crystals (25–2000 crystals), the heat of fusion was 40% larger than the bulk value. The melting temperature of the isolated single crystals was 123 ± 2 °C, 9 °C lower than that of the bulk material. We also measured the heat of fusion of quenched crystals (±15%) over a wide range of heating rates (20,000–100,000 K/s). Annealing the quenched crystals resulted in shifts in the endotherm peak by as much as 15 °C. © 2001 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 39: 1237–1245, 2001

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.