ABSTRACTHere we report a novel route for synthesizing nano-polycrystalline diamond (NPD) using stearic acid (C18H36O2) as a starting material under high pressure and high temperature. The obtained NPD shows a transparent dark-yellowish color similar to the standard NPD synthesized from graphite and consists of extremely fine diamond grains (∼10 nm). The temperature required for the present synthesis of pure transparent NPD is as low as 1000°C at 13 and 17 GPa, which is surprisingly lower than that for conventional NPD synthesis (1800–2000°C). The amorphous-like, extremely poorly crystalline graphite produced by the thermal decomposition of stearic acid likely provides preferential nucleation sites for diamond and significantly lower the activation energy. The removal of volatile components such as H2O generated through the decomposition from the system is a key to obtain pore-free transparent NPD. Magnesite, MgCO3 and periclase, MgO can be used as an efficient H2O remover through the hydration reaction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.