Abstract
The nanomechanical characteristics of polycarbonate (PC) polymer were investigated by atomic force microscope (AFM) and nanoindentation. Scratching, wear properties, hardness and Young's modulus were obtained. The relationships between scribing feed and speed, surface depth and roughness and applied load were also investigated. The results indicated that as the applied load was increased, the furrow depth and the surface roughness increased. When the scribing feed was increased, the depth and roughness decreased. Increasing the furrow speed also decreased the surface roughness. The applied load is more significant than the scribing speed on the material removal rate. In addition, the Young's modulus and hardness of the polycarbonate material were 1.8 and 0.2GPa, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.